ТЕХНИЧКИ ЛИСТ
02.12.2013

Fontecoat EP 80

 
Tikkurila Industry 9L
ОПИС A two component waterborne epoxy topcoat.
КАРАКТЕРИСТИКИ НА ПРОИЗВООДОТ Used as a topcoat in epoxy paint systems for steel surfaces.
Перпорачана употреба -

ТЕХНИЧКИ ПОДАТОЦИ
Features Resistant against modest mechanical and chemical stress.
Colour Cards Temaspeed Fonte tinting.
Gloss groups Gloss
Покривност

Recommended film thicknesses

Theoretical coverage

dry

wet

 

50 µm

105 µm

9.4 m2/l

80 µm

170 µm

5.9 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Разредувач Water
Mixing ratio Base 1 part by volume 169-series
Hardener 1 part by volume 007 1019
Метод на примена By airless spray or brush.
Pot-life (+23°C) 1½ h.
Drying times

DFT 70 µm

+ 15 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

4 h

2 h

1 h

Touch dry, after

8 h

5 h

2 h

Recoatable by itself, after

16 h

6 h

4 h

Fully cured, after

14 d

7 d

3 d


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation.
Содржина на цврсти материи 47 ± 2 volume % (ISO 3233)
61 ± 2 weight %
Густина 1,4 kg/l käyttövalmis seos.
Шифра на производот 169-series

ДЕТАЉИ ЗА ПРИМЕНА
Услови за примена All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below +15 ºC during application and drying. Relative humidity should not exceed 70 %. The surface temperature of the steel should remain at least 3 ºC above the dew point.
Припрема Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Priming Fontecoat EP 50 Beige and Temacoat GPL-S Primer.
Finishing Fontecoat EP 80.
Премачкување By airless spray or brush. If necessary, the paint can be thinned 0 - 10 %. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 140 - 180 bar. Spray angle shall be chosen according to the shape of the object.
Mixing of components First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use mechanical mixer for mixing.
Чистење на алатот Clean the spraying equipment immediately after use as follows:
1. Run the equipment with water to remove excess paint from the equipment.
2. Run the equipment with a mixture of approx 20% Thinner 1109 in clean water, at least two times.
3. Finally wash with undiluted Thinner 1109.

Wash the equipment with water before starting to paint again. Unwashed equipment can cause serious surface defects.

Contact Tikkurila Technical Service for detailed instructions for cleaning 2-component application equipment.
EU VOC 2004/42/EC ограничена вредност The Volatile Organic Compounds amount is 70 g/litre of paint.
VOC content of paint mixture (thinned by 10% by volume) 65 g/l.


КЛАСИФИКАЦИЈА ЗА БЕЗБЕДНОСТ И ЗДРАВЈЕ
во согласност со Регулативата (EC) No. 1272/2008
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj. For industrial and professional use only.
Safety data sheetFONTECOAT EP 80 [GB-ENG]
Hardener safety data sheetHARDENER 007 1019 [GB-ENG]
 
-


Назад