ТЕХНИЧКИ ЛИСТ
10.03.2009

Temadur SC 80

 
Tikkurila Industry 9L
ОПИС A two component gloss polyurethane paint, containing anticorrosive pigments, hardener aliphatic isocyanate.
КАРАКТЕРИСТИКИ НА ПРОИЗВООДОТ Recommended especially to be used as a single coat finish for agricultural and earth moving machinery and other machinery and equipment. Also suitable to be used as a topcoat in epoxy/polyurethane systems exposed to weathering and chemical stress
Перпорачана употреба Storage tank exteriors, steel framework and other steel structures.

ТЕХНИЧКИ ПОДАТОЦИ
Features Excellent weathering and abrasion resistance. A durable, easy to clean and non-chalking topcoat with good gloss and colour retention.
Colour Cards RAL, NCS, SSG, BS, MONICOLOR NOVA and SYMPHONY colour cards. TEMASPEED tinting.
Gloss groups Gloss
Покривност

Recommended film thicknesses/one coat application

Theoretical coverage

dry

wet

 

80 µm

125 µm

8.1 m2/l

120 µm

190 µm

5.4 m2/l

Recommended film thicknesses/as a topcoat

Theoretical coverage

dry

wet

 

40 µm

65 µm

16.2 m2/l

60 µm

95 µm

10.8 m2/l


Practical coverage depends on the application method, painting conditions and the shape and roughness of the surface to be coated.
Разредувач 1048 and 1067
Mixing ratio Base 5 parts by volume 532 series
Hardener 1 part by volume 008 7640
Метод на примена

By airless or conventional spray.

Pot-life (+23°C) 3 hours
Drying times

DFT 60 µm

+ 5 ºC

+ 10 ºC

+ 23 ºC

+ 35 ºC

Dust dry, after

2 h

1½ h

50 min

30 min

Touch dry, after

10 h

8 h

6 h

2 h

Recoatable, after

No limitations.


Drying and recoating times are related to the film thickness, temperature, the relative humidity of the air and ventilation. When oven drying is practised in temperatures + 50ºC - +100ºC, the evaporation time should be 5 - 30 minutes before ovening, depending on the wet film thickness and actual temperature.
Содржина на цврсти материи 65 ± 2 % volume (ISO 3233)
80 ± 2 % weight
Густина 1.4 ± 0.1 kg / l (mixed)
Шифра на производот 532 series

ДЕТАЉИ ЗА ПРИМЕНА
Услови за примена All surfaces must be dry. The temperature of the ambient air, surface or paint should not fall below + 5ºC during application or drying. Relative humidity should not exceed 80%. The surface temperature of the steel should remain at least 3ºC above the dew point.
Припрема Oil, grease, salts and dirt are removed by appropriate means. (ISO 12944-4)

Steel surfaces: Blast clean to grade Sa2½. (ISO 8501-1) If blast cleaning is not possible, phosphating is recommended for cold rolled steel to improve adhesion.

Zinc surfaces: Sweep blast clean with mineral abrasives, e.g. quartz sand, to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with PANSSARIPESU detergent.

Hot dip galvanized surfaces are recommended to be painted with a mist coat (paint thinned 25 - 30 %) before the actual priming.

Aluminium surfaces: Sweep blast clean with non-metallic abrasives to an even roughness. (SaS, SFS 5873) If sweep blasting is not possible, the surface should be roughened by hand abrading or washed with MAALIPESU detergent.

Note! Painted zinc and aluminium surfaces are not recommended when they are exposed to continuous condensation.

Primed surfaces: Oil, grease, salt and dirt are removed from the surface by appropriate means. Repair any damage to the primer coat. Note the overcoating time of primer. (ISO 12944-4)
Priming Temadur Primer, Temadur 20, Temacoat GPL-S Primer, Temacoat GF Primer, Temacoat HB Primer, Temacoat PM Primer, Temacoat GPL-S MIO, Temacoat RM 40, Temacoat SPA MIO, Temabond, Temaprime GF, Fontecryl 10, Fontecryl AP and Fontecoat EP Primer.
Finishing Temadur and Temathane.
Премачкување By airless or conventional spray. Airless spray: depending on the temperature of the components and shape of the object the paint can be thinned 0 - 15 %. Airless spray nozzle tip 0.011" - 0.015" and nozzle pressure 160 - 200 bar. Spray angle shall be chosen according to the shape of the object. In order to reach thicker coats (over 100 µm) use always "wet-in-wet" technique. At conventional spray the paint should be thinned 15 - 18 % to a viscosity of
20 - 25 s/DIN4.
Mixing of components First stir base and hardener separately. The correct proportions of base and hardener must be mixed thoroughly before use. Use Temaspeed Squirrel Mixer for mixing.
Чистење на алатот Thinner 1067 or Thinner 1048.
EU VOC 2004/42/EC ограничена вредност The Volatile Organic Compounds amount is 320 g/litre of paint.
VOC content in paint (thinned 18 % by volume) is 420 g/l.

КЛАСИФИКАЦИЈА ЗА БЕЗБЕДНОСТ И ЗДРАВЈЕ
во согласност со Регулативата (EC) No. 1272/2008
Containers are provided with safety labels, which should be observed. Further information about hazardous influences and protection are detailed in individual health and safety data sheets. A health and safety data sheet is available on request from Tikkurila Oyj.
Safety data sheetTEMADUR SC 80 [GB-ENG]
Thinner safety data sheetTHINNER 1067 [GB-ENG]
Hardener safety data sheetHARDENER 008 7640 [GB-ENG]
 
-


Назад